hello I would like to have a feedback regarding the below
I have a diaphragm wall which I am stabilizing using ground anchors. the grout specified must have 27 Mpa at 7 days before tensioning the cables.
The contractor is getting 18 Mpa at 10 days so he is not meeting the designer requirements.
I would like to know how much is critical the fact that the grout capacity is not being met ?
A ground anchor test will be done. If the results are OK, should I still be worried regarding the above ?