Hi everybody,
thanks in advance for any helpful hint.
Here's the question :
Have anyone ever experienced xray issue with a weld made with GTAW using a "Lift-Arc" start system.
Theory:
The tungsten electrode, at the ignition of the arc, would contamine the weld and make a xray-detectable defect.
Welding machine fabricator like Miller states that it is a "xray proof" system...
thanks in advance for any helpful hint.
Here's the question :
Have anyone ever experienced xray issue with a weld made with GTAW using a "Lift-Arc" start system.
Theory:
The tungsten electrode, at the ignition of the arc, would contamine the weld and make a xray-detectable defect.
Welding machine fabricator like Miller states that it is a "xray proof" system...