Dear Friends,
I qualified one PQR with GTAW+SMAW process as per ASME sec -9 for station piping work.In that Root & Hot pass with GTAW and remaining with SMAW. Please find given below PQR data
1. Test Coupon - 6 inch X 7.11 mm thick
2. GTAW Deposited weld metal in Root & Hot pass-4.22 mm
3.SMAW deposited weld metal thickness =7.11-4.22=2.89 mm
so in my WPS GTAW qualified weld metal thickness range is 8.44 mm as per ASME Sec-IX QW 451.1 and SMAW Weldmetal Qualified to weld 5.78 mm.
Please clarify,can i use this WPS to weld 2 inch X 5.54 mm thick pipe joints with full GTAW process?Its urgent.
I qualified one PQR with GTAW+SMAW process as per ASME sec -9 for station piping work.In that Root & Hot pass with GTAW and remaining with SMAW. Please find given below PQR data
1. Test Coupon - 6 inch X 7.11 mm thick
2. GTAW Deposited weld metal in Root & Hot pass-4.22 mm
3.SMAW deposited weld metal thickness =7.11-4.22=2.89 mm
so in my WPS GTAW qualified weld metal thickness range is 8.44 mm as per ASME Sec-IX QW 451.1 and SMAW Weldmetal Qualified to weld 5.78 mm.
Please clarify,can i use this WPS to weld 2 inch X 5.54 mm thick pipe joints with full GTAW process?Its urgent.