Sjscat
Industrial
- Jan 5, 2023
- 3
Hi,
I am new to this forum, but I have a question about heat treating 13-8 stainless. I am used to H950 being used to heat treat 13-8. However, I saw a call out for heat treating 13-8 parts to H900. I know H900 is used to treat 17-4 stainless.
I suspect H900 treatment, instead of H950, would increase 13-8 parts a few hardness points. Is this true? What other effects on the metal would be seen? I have found no information in regard to this. Can someone comment please?
Thanks!
I am new to this forum, but I have a question about heat treating 13-8 stainless. I am used to H950 being used to heat treat 13-8. However, I saw a call out for heat treating 13-8 parts to H900. I know H900 is used to treat 17-4 stainless.
I suspect H900 treatment, instead of H950, would increase 13-8 parts a few hardness points. Is this true? What other effects on the metal would be seen? I have found no information in regard to this. Can someone comment please?
Thanks!