sujit123

Materials
Mar 25, 2002
2
hardfacing welding upon gray cast iron
 
Replies continue below

Recommended for you

Check with Lincoln Electric or run a Google search for hardfacing electrodes, check Thomas Register
 
I recommend Magna 777 electrode best for all cast iron repairs. it is very easy in use, and no pre-heating required.
 