Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Hardness test for boiler pressure parts welded portion?

Status
Not open for further replies.

jba15

Mechanical
Sep 13, 2015
2
Hi,

I would like to inquire if when are we gonna apply hardness test for boiler pressure parts. We will replace final superheater stub tubes (SA213-TP347H).

Good day.

jba15
 
Replies continue below

Recommended for you

?

What does your contract require?
What does your customer require?

When will it happen? We don't know your job's schedule. 8<)
 
Generally there are no hardness test requirements for 347H boiler tube welds. but review racookpe1978.
 
We required that the stub tubes be replaced, and that the tubes be heat treated after welding works (PWHT). Then it will be checked by Phase Array UT, MT, and PT. Make repairs based on the result.

The contractor only required for the supply of new tubes.

We planned to implement the replacement during our planned maintenance schedule in November 2015. Approximately 20 days period.

Also, in addition, does MT works for SA213-TP347H material? I cannot verify it now, not until the boiler unit is shut down.
 
Status