deco0404
Mechanical
- Nov 3, 2009
- 79
Guys,
we just ran some production test plates as part of our current welding project.
On one of the samples the hardness results are a little high. We have one reading (out of 45) which is 378Hv. Our max allowable is 350Hv. We are working to DNV C401.
My query; There were 3 readings taken in this particular location (weld HAZ), the average of the 3 readings is 314Hv. I have done hardness testing down the years, and as it is quite a subjective test, we have always worked on average readings, and not individual readings.
Does my test plate pass the test or not?
regards
Declan
we just ran some production test plates as part of our current welding project.
On one of the samples the hardness results are a little high. We have one reading (out of 45) which is 378Hv. Our max allowable is 350Hv. We are working to DNV C401.
My query; There were 3 readings taken in this particular location (weld HAZ), the average of the 3 readings is 314Hv. I have done hardness testing down the years, and as it is quite a subjective test, we have always worked on average readings, and not individual readings.
Does my test plate pass the test or not?
regards
Declan