Hi all, a project engineer is offering me a hastelloy piping system connecting to some ~15 foot dia x ~15 foot tall buffer tanks. He says that the most economic solution is to build the tanks from plastic or plastic/grp rather than metallic construction. He says not to use plastic piping due to the possibility of erosion from particles in the liquid. I have no experience of combining metal piping and plastic tanks. Is it an OK thing to do? Thanks all!