1)I would like to know advantages and disadvantages of using HCl or SO4H2 for the regeneration in a demineralization water plant.
2) How can I make an economical evaluation from the point of view of chemicals consumption ?
3) Is it possible to use our actual SO4H2, Carbon Steel tank to store the HCl?, Which should be the best suited material for the HCl.
4) The mixed bed vessel have distributors made of SS AISI 316L are they good for HCl or we have to change the material.
Actually we are processing an average of 180 m3/hr of water in the cation-anion exchangers and our consumption of Sulfuric acid 98% is 560 lts per regeneration.
In the mixed beds we are processint an average of 300 m3/hr of water and we are consuming 360 lts. of sulfuric acid 98 % per regeneration.
Thanks in advance for any help
2) How can I make an economical evaluation from the point of view of chemicals consumption ?
3) Is it possible to use our actual SO4H2, Carbon Steel tank to store the HCl?, Which should be the best suited material for the HCl.
4) The mixed bed vessel have distributors made of SS AISI 316L are they good for HCl or we have to change the material.
Actually we are processing an average of 180 m3/hr of water in the cation-anion exchangers and our consumption of Sulfuric acid 98% is 560 lts per regeneration.
In the mixed beds we are processint an average of 300 m3/hr of water and we are consuming 360 lts. of sulfuric acid 98 % per regeneration.
Thanks in advance for any help