Hi! We design HDPE Stubend(s) for use of HDPE Lined carbon steel pipelines application. We provide stubend collor thickness (flange face thickness) double of pipe thickness. In recent conversations, we came to knew stubend flange face thickness 1 to 1.5 times of pipe thickness is sufficient.
We would like to know what will be the idle flange face thickness or flange dimensions without effecting the application. (HDPE lined carbon steel pipelines or spools) Photo of HDPE Stubend attached for reference.
Also let us know what will be %of compression on HDPE flange face thickness during tightening.
Thanks in advance.