Hello all not been in a wile hope everyone is doing okay, hoping that someone can help me with a question if you have Weld pipe to plate will that cover you in plate to plate if yes or no please explain the reason for this

Thanks for your time
 
Draw a diagram and attach it to a post.
 
If I remember correctly 24" diameter pipe is considered plate,
according to AWS D1.1.
 
Are you qualifying a welding procedure or a welder and to which Code?
 
Hi weldstan it will be a PQR I should have asked the question a bit better to be honest if I was to use a 30mm die bar to a 30mm plate would that also qualify for a plate to plate joint I know that if you use 30mm thick it will take you from 5mm and anything grater according to 15614-1
 
30 mm thick bar has a "wall thickness" of 15 mm, giving a range from 3 to 30 mm from pipes dia 15 mm to infinity (= plates).
 
Kingnero thanks, can you explain why pipe dia 15mm to infinity =plates please, I know that a butt Weld in plate covers in pipe over 500mm or 150 mm rotation position if you can explain my question that would be great

Thank you
 
See table 9. Can't get more clear than that.
 
Kingnero thank you
 