HELP!!! A217 WC6 Cast low phosporus content!!!

Status
Not open for further replies.

pedroluis81

Chemical
Nov 24, 2009
1
Hi,

Does anyone know a foundry that can supply an ASTM A217 WC6 with a phosporus content less than 0.011%?

Several foundries have delined due to this...

This is for a valve manufacture.

Thanks a lot!
 
Replies continue below

Recommended for you

Try the Japanese. They have a history of being able to hold tight metallurgical tolerances when making steel.
 