HELP HELP ME,
I have a big problem, I met corrosion under insulation CUI on external
vessel (cigar) storage GPL PC: 279 PSI, severe external corrosion
under insulation
Nominal thickness: 33.33 mm (1 5/16 '') and minimum requirements:
31.70 mm (1.248 '') and CA: 1.6 mm (0.0625 '') pfrofondeur of craters
from 2mm to 4mm more places furrows / corrosion slinger lines 5.3 mm
tell me how to fix and that applies to API 510 or API MAWP 579 FFS
The API also allows recharging 510 to 50% t required
 