Dec 21, 2004 #1 nugent01 Materials Dec 14, 2004 1 0 0 US Im looking for any kind of information on initial and final set of concrete..I realize this varies from mix to mix but are there any standard times you can reference? Thanks...
Im looking for any kind of information on initial and final set of concrete..I realize this varies from mix to mix but are there any standard times you can reference? Thanks...
Dec 21, 2004 2 #2 fepc Structural Oct 27, 2004 19 0 0 Look at "Design and Control of Concrete Mixtures" by PCA. It depends on temperature, design mix , etc. Upvote 0 Downvote
Look at "Design and Control of Concrete Mixtures" by PCA. It depends on temperature, design mix , etc.
Dec 21, 2004 1 #3 SlideRuleEra Structural Jun 2, 2003 5,528 0 36 US Here are some online resouces (free .pdf downloads) ftp://imgs.ebuild.com/woc/C00I046.pdf ftp://imgs.ebuild.com/woc/C99G029.pdf ftp://imgs.ebuild.com/woc/C970011.pdf ftp://imgs.ebuild.com/woc/C920523.pdf ftp://imgs.ebuild.com/woc/C920126.pdf ftp://imgs.ebuild.com/woc/c900541.pdf ftp://imgs.ebuild.com/woc/c900287.pdf Upvote 0 Downvote
Here are some online resouces (free .pdf downloads) ftp://imgs.ebuild.com/woc/C00I046.pdf ftp://imgs.ebuild.com/woc/C99G029.pdf ftp://imgs.ebuild.com/woc/C970011.pdf ftp://imgs.ebuild.com/woc/C920523.pdf ftp://imgs.ebuild.com/woc/C920126.pdf ftp://imgs.ebuild.com/woc/c900541.pdf ftp://imgs.ebuild.com/woc/c900287.pdf