Can anyone help me with a material thickness and weld size on the following problem.
I have to hydrotest a 12" Sch 160 P91 Pipe Spool. The spool has machined Buttweld ends. In the past the company has plugged the pipe internally with a 1 1/2" thick plate and welded it in place with a 2" fillet weld. I would like to confirm that this is ok mechanically, but I'm not sure how to calculate minimum plate thickness or minimum fillet size.
The Hydrotest pressure is 5055 psig.
Any help would be greatly appreciated.
IAM
I have to hydrotest a 12" Sch 160 P91 Pipe Spool. The spool has machined Buttweld ends. In the past the company has plugged the pipe internally with a 1 1/2" thick plate and welded it in place with a 2" fillet weld. I would like to confirm that this is ok mechanically, but I'm not sure how to calculate minimum plate thickness or minimum fillet size.
The Hydrotest pressure is 5055 psig.
Any help would be greatly appreciated.