I have recenntly become involved in a Hepa filtration project and am having numerous "seal"failures when the units have been installed on site. The filters are equipped with a gel seal and knife edge. These however seem to be the source of the leaks. New gel seals have been installed with improved but similar failures. Are the other factors that can cause these gel seals to fail? Just seaching for ideas as i am out of repair ideas and the manufacture is currently of little help.