Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Hi Engineers How to weld clean ou

Status
Not open for further replies.

MA69

Mechanical
Jan 5, 2022
4
Hi Engineers
How to weld clean out door base plate with annular plate? What is the welding procedure?
 
Replies continue below

Recommended for you

Whatever the materials and use case suggests...

Dan - Owner
Footwell%20Animation%20Tiny.gif
 
This is an API Storage Tank question ... Suggest that you post in "Storage tank engineering" forum

MJCronin
Sr. Process Engineer
 
I don't remember if there is any additional detail on that in API-650. But it may simplify things, at the cost of some material, to extend the base plate in as far as the annular plate.
 
I attached the photos of COD our API 650 Storage tank.
Tank Details:
Dia : 200 ft
Height : 48 ft
COD Base plate Thickness : 34mm
Annular plate Thickness ; 14 mm
As in our case, we are going to only replace the bottom reinforcement plate (or annular plate) of the clean out door.

Does we have to stress-relief the whole clean-out door assembly afterwards? or just PWHT of the new welding of the new annular plates to the new door reinforcement plate?

Or, in this case, is not required.

Please advise me.
 