Hi. I have some problem on bagging

Status
Not open for further replies.

PhenolicComp

Aerospace
Nov 8, 2019
1
Hi. I have some problem on bagging my phenolic resin. It always blow up during autoclave cure. Anyone have the same issue? Any ideas ob how to properly bag phenolic resin? Thank you.
 
Replies continue below

Recommended for you

I suggest asking to delete this thread and posting here -> forum327
You're more likely to get better responses.

"Know the rules well, so you can break them effectively."
-Dalai Lama XIV
 
I don't do that forum. You probably need to de-aerate your resin before use by ultrasonic shaking under a vacuum.