itsleighton
Civil/Environmental
I have a jobsite in which the water table is very high (9ft) The project required ecxcavating 38 feet deep and stockpiling the material onsite for 2 months. Even with dewatering wells, the water does not fall out of the soil so it stays vary saturated. The stockpiled material is also still very moist even at the very top. When compacting this material for backfilling, we are getting roughly 90-94% maximum density, but with 6-8% moisture content. What is expected of the behavior of the soil if it is backfilled with that high of moisture if the existing surrounding ground contains an even higher moisture content naturally? The project is a lift station with the bottom of the wet well sitting on shale, so it wont settle. The valve vault is sitting at approximately 9ft down from the top of ground which will be placed on backfilled material. will this ground settle?