HazGas
Chemical
- Oct 26, 2005
- 11
I have been hired to do some safety engineering work. In my exploration of the work site I have found numerous high pressure (up to 6000 psig) flex hoses without restraints. These are high quality stainless convoluted or stainless/PTFE hose, but many are decades old. They receive a visual inspection yearly but that doesn't mean much to me. My experience is that these inspections are pencil whipped.
I have suggested they immediately implement a requirement to install restraints on hoses being used at 150 psig or more. (This is the industry standard.) It has been met with a little resistance by those resistant to any changes. So I need to prove to these guys how serious this isse
can be.
I know I've seen an old video from the '60s where a high pressure stainless hose about 20' long fails and proceeds to destroy absolutely everything around it, including smashing cinder block walls. All the videos I can find on the Internet show hydrostatic failures, pull test failures, restraints actually working, or the gas being shut off immediately after failure (which wouldn't happen in a real failure.)
Has anyone else seen this video or know where I
might be able to get it? Or something similar? Thanks!!
I have suggested they immediately implement a requirement to install restraints on hoses being used at 150 psig or more. (This is the industry standard.) It has been met with a little resistance by those resistant to any changes. So I need to prove to these guys how serious this isse
can be.
I know I've seen an old video from the '60s where a high pressure stainless hose about 20' long fails and proceeds to destroy absolutely everything around it, including smashing cinder block walls. All the videos I can find on the Internet show hydrostatic failures, pull test failures, restraints actually working, or the gas being shut off immediately after failure (which wouldn't happen in a real failure.)
Has anyone else seen this video or know where I
might be able to get it? Or something similar? Thanks!!