Hi,
I'm looking for a suitable material, composite or layered sheet for replacing an LCD overlay, currently made of glass, with the ultimate goal of significant weight reduction.
Normally, a hard coated PMMA sheet would do the job in most applications and the weight would be cut in half. However, in this particular product, I need extra stiffness to prevent (or minimize) external factors bending the sheet and reaching the LCD, possibly damaging it.
Glass is about 10-20 times stiffer than any plastic I know of and I'm not expecting to even come close to that. Worst scenario is ending up with the aforementioned PMMA; however, I'd like to know that at least I'm using "the best" there is. Cost is not an issue.
Any suggestions? Thank you!
I'm looking for a suitable material, composite or layered sheet for replacing an LCD overlay, currently made of glass, with the ultimate goal of significant weight reduction.
Normally, a hard coated PMMA sheet would do the job in most applications and the weight would be cut in half. However, in this particular product, I need extra stiffness to prevent (or minimize) external factors bending the sheet and reaching the LCD, possibly damaging it.
Glass is about 10-20 times stiffer than any plastic I know of and I'm not expecting to even come close to that. Worst scenario is ending up with the aforementioned PMMA; however, I'd like to know that at least I'm using "the best" there is. Cost is not an issue.
Any suggestions? Thank you!