Hi guys!
I have made a FEM analysis of a roller and the results show below.
The forces acting are flexion and torsion. The diameter max. of the roller is 330 mm and 5000 mm of total length.
I do not like high stress values in the fillet zone. I tried refine mesh but the values increase even more. Also I tried increase fillet radius but there is not change.
Is something wrong? Or only generates a hardening for localized plastic deformation and i can ignored this?
I would like to know what you think
Thanks
Sebastian.
Zoom image:
"Persistence prevails, like a stream that is temporarily blocked by boulders and then collects force enough to overflow onward."
I have made a FEM analysis of a roller and the results show below.
The forces acting are flexion and torsion. The diameter max. of the roller is 330 mm and 5000 mm of total length.
I do not like high stress values in the fillet zone. I tried refine mesh but the values increase even more. Also I tried increase fillet radius but there is not change.
Is something wrong? Or only generates a hardening for localized plastic deformation and i can ignored this?
I would like to know what you think
Thanks
Sebastian.


Zoom image:

"Persistence prevails, like a stream that is temporarily blocked by boulders and then collects force enough to overflow onward."