Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

High Temperature Ball Valves

Status
Not open for further replies.

Charlesan

Industrial
Apr 23, 2008
8
Got an application for high temperature ball valves, design temperature 550C,used on gases hydrogen, ammonia also needs to meet full vacuum shutoff, any ideas for starters?
 
Replies continue below

Recommended for you

Not sure about the Hydrogen pressure, but most likely it will be auto-ignited upon leakage due to operating temperature.
Extra attention on sealing material/quality is highly suggested.
Graphite packing usually consist of graphite (93 to 99% purities) with bonding agent such as Zinc, PTFE, etc. Please note that Zinc start to become permeable above 200 degC and PTFE above 210 degC. These numbers often differed or debated amongst packing supplier and end-user.
Therefore I would suggest to choose the purest graphite possible.
Not all TapcoEnpro, JamesWalker, ERIKS, etc. sealing components are suitable for high temperature application. Ask for burning and/or aging test result if possible.

I had some incidents on 93% graphite being exposed to 480degC and showing gland extrusion/intrusion after only several cycles.

Companies mentioned above by Tbe Obturator and TugBoat are quite ok. IMI group (they have acquired some ball valve companies) are worth considering as well.

Regards,
D


 
Ladish & ValvTechnologies also both make metal-seated ball valves for this, depending on valve size & metallurgy you need.
 