Does anyone have section properties for a C15x45 channel from 1935?

The AISC Rehab and Retrofit Guide doesn't cover channels, and the oldest Steel Manual I have access to is from 1946, which only has C15x33.9, C15x40 and C15x50 sections (identical to today's sections).
 
Replies continue below

Recommended for you

Thanks, exactly what I needed.
 
1932 AISC Steel Construction manual has the same thing on page 35.

Mike McCann
MMC Engineering
Motto: KISS
Motivation: Don't ask
 
Hey connectegr...can you post a pdf that shows the properties of a C12x25. Your other page with the 15 inch channels has been really helpful but I think I might need the page before. Thanks!
 