tliebhold
Structural
- Aug 16, 2011
- 6
I'm involved in the remodel of a building that was built under the AISC 8th edition (built in 1983), where the strength of steel studs for composite action is given by a table, as opposed to a formula. With the remodel I need to check the composite beams under current code, which is, in part, based upon the grade of the shear studs. Does anyone know what the typical steel grade of studs was at this time?
Thanks.