The shop I work for is currently had this question came up about; is there anything specific in Code that says how big a hole can be when compared to the nozzle that will go in that hole. For instance a 2" pipe, OD is 2.875" the hole diameter that was cut is say 3.5" is there anything in code that says you just cant weld that up with that big of a gap. I know in our case some welders would try and some would notify someone of this situation...
 
Replies continue below

Recommended for you

Well, first, 2" pipe is 2.375" o.d. but it really doesn't matter.

i don't remember this being addressed in code. BUT, the gaps at welds must meet your wps.
Most wps do not stretch out to 7/16" weld gap.
 
However, you can build up the hole with weld metal, NDE (hopefully) and then re-bevel etc as required. Approved procedures of course.