PowersPE80
Civil/Environmental
- Apr 27, 2012
- 10
Hello. I was surveying a 3-story, terra cotta building with stucco exterior. The building has plenty of random hairline cracks, apparently due to shrinkage. At the bottom corner of one of the windows there is a horizontal crack, approximately 8'-10' long, located directly at the bottom corner of the window. (See the attached picture). Is this from the stucco shrinking? or the terra cotta shrinking and therefore cracking the stucco? Or a combination of both? There is a similar crack at the window in the same location on the first and second floors. Any thoughts would be greatly appreciated. Thanks.