Dec 17, 2015 #1 fakhfakh Industrial Nov 11, 2004 48 0 0 TN Dear All, Is it prohibited by ASME Section VIII Div1 that a repad be formed at a temperature 300 to 400°C ? This repad SA516Gr70 will reinforce an opening at the knuckle of the head of a pressure vessel. The complete PV will be subjected to PWHT per UCS-56
Dear All, Is it prohibited by ASME Section VIII Div1 that a repad be formed at a temperature 300 to 400°C ? This repad SA516Gr70 will reinforce an opening at the knuckle of the head of a pressure vessel. The complete PV will be subjected to PWHT per UCS-56
Dec 17, 2015 #2 Don56 Mechanical Feb 18, 2015 203 0 0 US It is not prohibited. Since you are performing PWHT fiber elongation is not a problem. Upvote 0 Downvote