I am estimating the time it will take to burn 1lb of commercially pure ti powder in oxygen (outside atmosphere)? Thanks
 
Replies continue below

Recommended for you

Titanium is supposedly relatively slow burning when not dispersed. While there was presumably a lot of total energy in the burn, it would not have been until the last 1/2 minute or so that the steel would have been exposed to anything close to a melting temperature, and the exposure was probably too brief.

TTFN

FAQ731-376
 
If you just want to burn a hole in the lid use Thermite.
 