B31.3 and ASME Section VIII indicates SA-105 material(for a flange, in this case) has a MDMT of -20 F. However, B31.3 allows for some materials to be used as low as -155 F without impact testing (Table 323.2.2, note 3) provided the stress ratio does not exceed 0.3. The service is propane refrigeration (Normal Fluid Service). The question is whether or not "note 3" is applicable to SA-105 flanges? 'course, we'll need to make sure the bolts are good for the lower temp, too, if the flange is OK to -155 F.
Any feedback would be greatly appreciated.
Any feedback would be greatly appreciated.