I want to get many (up to three) PWHT (1 hour stress relief at 1150°F or per ASME Sect.8 div.1 - UCS-56) on a pressure vessel shell (SA-516-70N) without deterioration of the mechanical properties below a specified limit.
-Is there a variable (chemical composition, metal structure, dimensions, holding time of the PWHT, etc) which does influence the repeatability of a PWHT (stress relief)?
-How many times can I repeat the same PWHT?
Regards
I want to get many (up to three) PWHT (1 hour stress relief at 1150°F or per ASME Sect.8 div.1 - UCS-56) on a pressure vessel shell (SA-516-70N) without deterioration of the mechanical properties below a specified limit.
-Is there a variable (chemical composition, metal structure, dimensions, holding time of the PWHT, etc) which does influence the repeatability of a PWHT (stress relief)?
-How many times can I repeat the same PWHT?
Regards