Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How thick can a riveted joint get.

Status
Not open for further replies.

ChasGen61

New member
May 15, 2012
6
How thick can a riveted joint get. Let's say we have 2 aluminum sheets(2024-T3)being riveted with AD5 rivets. Assume both sheets are equal in thickness and thick enough so that we are shear critical. How thick can both sheets get using rivets? If you answer this where can I reference it?
 
Replies continue below

Recommended for you

Hi Chas,

A rough guide for solid rivets is:

• The rivet diameter, D, should be equal to or greater than the thickness of the thickest part in the joint and less than 3 x the thickness of the thinnest part.
• If the stack-up (assembly thickness) exceeds 2,5 x D, the rivet diameter should be increased, or another type of fastener used, such as a Hi-Lok or lock bolt.
• Where fluid tightness is essential the stack-up should not exceed 2D. This is because a bigger stack-up will require a larger force in the joint to ensure sealing, which may not be readily attainable.
The info comes from a well-known, large US Aerospace Corporation

Andries


 
if you consider the bending you're imposing on the rivet, then you can go further than 2D, but i think they'll quickly become ineffective and you'll move to Hi-Lites/Hi-Loks.
 
Try FAA Advisory Circular 43.13.

In theory, there is no difference between theory and practice; experience suggests that in practice, there is.
 
going back to the original question, -5 rivets are shear critical at thickness = 0.063" (depending of course on the sheet material), so being greater than this doesn't really define the problem ... a stack up of 1.5D to 2D (0.3") wouldn't raise questions ... what stack up are you considering ?
 