ChFa
Automotive
- May 17, 2016
- 2
Hello, everyone, I have a question on how to avoid crevice corrosion. I wanted to measure the pitting potential of stainless steel with welding seam. The exposure area (1 cm2)is fixed by the cell. However, crevice corrosion always occured near the seam. Do you have any good advices to avoid the crevice corrosion?