C.Amini
Mechanical
- Oct 20, 2017
- 18
Hello everyone
I am modeling FSW ( friction stir welding). I already simulate it using the tool that had no pin only including shoulder.
Lately I wanna simulate the process with tool including shoulder and pin which should penetrate 5.6mm but my simulation became divergent after penetration of 2.1mm . and some times these errors arise during solution:
1- Some of the element based thermal loads may be inappropriate. Check
applied element loads carefully. Ensure that film coefficients and
bulk temperatures are always positive.
2-Element 11310 (type = 1, SOLID226) (and maybe other elements) has
become highly distorted. Excessive distortion of elements is usually
a symptom indicating the need for corrective action elsewhere. Try
incrementing the load more slowly
how can i adjust options of contact element or some options of solution to achieve high penetration (5.6mm) and avoid divergence
any comment would be helpful and appreciated
regards
cyrus
I am modeling FSW ( friction stir welding). I already simulate it using the tool that had no pin only including shoulder.
Lately I wanna simulate the process with tool including shoulder and pin which should penetrate 5.6mm but my simulation became divergent after penetration of 2.1mm . and some times these errors arise during solution:
1- Some of the element based thermal loads may be inappropriate. Check
applied element loads carefully. Ensure that film coefficients and
bulk temperatures are always positive.
2-Element 11310 (type = 1, SOLID226) (and maybe other elements) has
become highly distorted. Excessive distortion of elements is usually
a symptom indicating the need for corrective action elsewhere. Try
incrementing the load more slowly
how can i adjust options of contact element or some options of solution to achieve high penetration (5.6mm) and avoid divergence
any comment would be helpful and appreciated
regards
cyrus