Hi,
I am modelling tensile dog bone specimen. I manage to simulate until before it neck..After that, i dont know..i read through the manual that we have to set damage model..for instance using Damage for ductile materials..However, the problems arise..how to measure stress triaxiallity,fracture strain and strain rate?..please anybody help me. The material is steel. Or maybe other suggestions?
I am modelling tensile dog bone specimen. I manage to simulate until before it neck..After that, i dont know..i read through the manual that we have to set damage model..for instance using Damage for ductile materials..However, the problems arise..how to measure stress triaxiallity,fracture strain and strain rate?..please anybody help me. The material is steel. Or maybe other suggestions?