AjSCCMelt
Industrial
- Dec 2, 2022
- 13
thread330-428846
Dear all,
We just started casting duplex stainless steel castings (ASTM BPVC II A SA-995).
We have a 500kgs medium frequency induction furnace.
CASE 1:
We casted a ring like casting (impeller casing wearing ring) in ASTM BPVC II A SA-995 Grade 4A and all the mechanical and chemical properties where achieved but the casting developed pin holes even after taking precautions in moulding, melting and even after manual argon purging the pouring laddle with a lancing pipe (Although the amount of pin holes where hugely reduced as compared to standard manufacturing process).
CASE 2:
We casted a flange in ASTM BPVC II A SA-995 Grade 2A and achieved chemical composition as per standard but the casting cracked after heat treatment also the mechanical properties where not achieved by a huge margin.
Questions:
FOR CASE 1:
1. What should i do to get rid of pin holes.
2. Melting temp. at which metal is poured in laddle.
3. Improvement in argon purging that i could carry out.
FOR CASE 2:
1. Why does the casting cracks even after heat treatment according to standards?
2. Why does the mechanical properties are achieved in GRADE 4A but are far from standard in GRADE 2A?
Thanks and waiting for your valuable suggestions.
Dear all,
We just started casting duplex stainless steel castings (ASTM BPVC II A SA-995).
We have a 500kgs medium frequency induction furnace.
CASE 1:
We casted a ring like casting (impeller casing wearing ring) in ASTM BPVC II A SA-995 Grade 4A and all the mechanical and chemical properties where achieved but the casting developed pin holes even after taking precautions in moulding, melting and even after manual argon purging the pouring laddle with a lancing pipe (Although the amount of pin holes where hugely reduced as compared to standard manufacturing process).
CASE 2:
We casted a flange in ASTM BPVC II A SA-995 Grade 2A and achieved chemical composition as per standard but the casting cracked after heat treatment also the mechanical properties where not achieved by a huge margin.
Questions:
FOR CASE 1:
1. What should i do to get rid of pin holes.
2. Melting temp. at which metal is poured in laddle.
3. Improvement in argon purging that i could carry out.
FOR CASE 2:
1. Why does the casting cracks even after heat treatment according to standards?
2. Why does the mechanical properties are achieved in GRADE 4A but are far from standard in GRADE 2A?
Thanks and waiting for your valuable suggestions.