Jul 24, 2006 #1 TAGE Mechanical Feb 24, 2003 25 0 0 TH Dear Sir Does anyone have any idea about the normal (suitable) material for the HRSG stack silencer or so called "buffer" installed INTERNALLY inside the stack? Please share me your experience regarding this matter. Thanks for your kind help Best Regards
Dear Sir Does anyone have any idea about the normal (suitable) material for the HRSG stack silencer or so called "buffer" installed INTERNALLY inside the stack? Please share me your experience regarding this matter. Thanks for your kind help Best Regards
Jul 25, 2006 #2 MJCronin Mechanical Apr 9, 2001 5,086 0 36 US TAGE If the temperature is less than about 550F, 304 SS should be suitable. I have encountered thin walled SS liners used in power generating service -MJC Upvote 0 Downvote
TAGE If the temperature is less than about 550F, 304 SS should be suitable. I have encountered thin walled SS liners used in power generating service -MJC