I would appreciate some input from the corrosion engineers here. If i have hydrogen gas flowing into a vessel, can it dissociate into atomic hydrogen and lead to hydrogen embrittlement, or does the hydrogen already have to be in atomic form (i.e. be the result of a corrosion reaction)? All input is welcome!
 
Replies continue below

Recommended for you

Metals, such as iron, can absorb gaseous hydrogen through chemisorption.
 
Thank you for the links and suggestions, they have been very helpful.
 
By the look of that carbon steel is ill-characterised (not really known) for hydrogen damage by hydrogen gas(that's embrittlement plus blistering). Is any metal for typical applications?

Use translation assistance for Engineers forum

Note the rules include No Student posting
 