I want to now if it's possible to reverse the process of esterification of glicerol of hidrogenated rosin ? How ?

Thanks

 
Replies continue below

Recommended for you

Is it possible to reverse the esterification of ... what?
That is, you are trying to produce what? from what??
What is your goal? Perhaps clarifying the question and providing more info will help.
Cheers, and good luck.
 
I'm not exactly sure what you are asking, but the simplest way to undo an ester is via saponification. If you can be more specific as to what your ester is and what you are concerned with recovering (alcohol, fatty acid or both) I can give you far more specific instructions.
 