We have to hydrotest a heat exchanger, this exchanger used as ethylene vaporizer at -104C. This exchanger hydrotesting with methanol before which is not available now. Thus we are considering other mediums for hydrotest fluid. One idea floating around is to use nitrogen. I would like to know if anyone out there has expeience with hydrotesting in cryogentic area and if you have any suggestions.
Thanks.