Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

hydrotest ASME procedure,

Status
Not open for further replies.

NOURIALI

Industrial
Joined
Aug 15, 2019
Messages
5
Location
US
Hi all,
I am making a hydrotest console to test 60 inches long 8" diameter SS tubing @ a test pressure of 800 PSI,
I'll appreciate if you can help in elaborating a plan that lays down all standards steps, ASME standards and requirements.
thanks
 
Are you testing a few of these or hundreds?
You have the pertinent sections of the Code, don't you?
What part of the Code are you trying to meet?
Is this 8" OD or 8pipe?

In general you need:
An approved procedure
Clean water (no Cl, low TDS)
End caps/plugs rated to the pressure
The ability to fill the pipe while assuring all air is removed
Pump up to needed pressure
Isolate from pressure source and monitor pressure decay for the required time
Release/drain valve and way to capture and reuse water (as long as it is still clean)
A way to dry the pipe sections

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Many thanks,
a few for now,
the ID is. 8",
my target is to make a technical plan. to submit with documents,
I did not look yet for any standards, I wanted first to have an idea on how such a project is approached by professionals in this field as far as standards goes,
first time doing this, I'm not sure where to start,
thanks for the general do-list.
we have a test console that we will be using. my problem is to write a procedure that will abide by standards requirements.
thanks,
 
Why are you even doing this though? For something like this just employ a test house or testing company who have all the equipment and procedures and the they give them to you. Far cheaper than making something.

The other things missing form the list though is temperature measurement (especially if the test is for more than a few minutes) and pressure relief to avoid over pressurising your test piece accidentally.

But 8" diamter tubing?? That sounds very big for "tubing"

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 