I have problem with leakage in Raw water pond lining with 1mm.HDPE SHEETwith welding joint type. My pond was 90 m. by 45 m.water level is 3.5 m. The water level is lower 1.2 mm./hour which is 2.88 cm/day. My point is we cannt find the criteria that this is accepatble for such kind of this linning or not.
Does anyone out there has experience with acceptance criteria of this HDPE sheet. Is there any sources that I can reference to?.
My Site condition : avg.temp 32deg.c(dry bulb), Humidity 70% wind 3m/s dew point 20deg.c
Thanks
Does anyone out there has experience with acceptance criteria of this HDPE sheet. Is there any sources that I can reference to?.
My Site condition : avg.temp 32deg.c(dry bulb), Humidity 70% wind 3m/s dew point 20deg.c