i would like to know if anyone has undertaken the study of equipment used in preheating die prior to diecasting (gravity not pressure.

i am intrested in efficiency of gas v electric, pros and cons etc
 
Replies continue below

Recommended for you

In the August 2002 issue of JOM, there is an article titled Simulating Convective Die Heating for Forgings and Pressure Casting written by a company that makes heaters. This article, plus its references, would be a starting place.
 