Identification of quench cracks at tooth root

Status
Not open for further replies.

UCengno1

Mechanical
Sep 22, 2005
70
I have a small gear, 26 DP / 46 teeth, fabricated from 8620. A recent gear tooth failure problem was potentially linked to the existance of quench cracks. I question the observation only on the basis that only a single tooth was found to be cracked. Seeing as the entire gear would be submitted to the same heat treatment wouldn't I expect other teeth to exhibit the quench cracks? Comments?

BCK
 
Replies continue below

Recommended for you

Where did the tooth fail and what is the orientation of the suspected quench crack relative to the tooth fracture?
 
"..... only a single tooth was found to be cracked."

Was it inspected with wet magnetic particle ?
Did the magnafluxer check it in several steps, with a new magnetization for each orientation?
 
After additional inquiry I am finding some hesistancy from the metallurgist regarding the initial failure diagnosis, e.g. not all teeth were checked just the ones near the failure point, not sure if it is a quech crack, etc... Is it possible to look for some heat treat residual material in the crack to determine if it appeared during quench?
 
You can examine the fracture with a scanning electron microscope (SEM)and determine if there is intergranular fracture at the crack initiation. Quench cracks are intergranular; fatigue cracks are not. Overload fracture, especially in a carburized case, may exhibit some intergranular fracture in the heavy portion of the case, but near the intiation point, the fracture should be a predominantly quasi-cleavage.
 
swall,

Thank you for the very helpful guidance. [2thumbsup]