Hey all,
I'm trying to identify a JIS spline off a Yamaha R6 output shaft.
Below are some basic spline specs which I was able to measure, I have also attached a photo of the female spline profile.
13 spline
Major Diameter - ~24.7mm
Minor Diameter - ~21.0mm (difficult to accurately measure due to odd number of splines)
I can provide more measurements if needed.
If anyone would be able to help identify which JIS spline spec this is, it would be greatly appreciated.
End goal of this would be to get a DXF and EDM the spline profile.
Thanks!
I'm trying to identify a JIS spline off a Yamaha R6 output shaft.
Below are some basic spline specs which I was able to measure, I have also attached a photo of the female spline profile.
13 spline
Major Diameter - ~24.7mm
Minor Diameter - ~21.0mm (difficult to accurately measure due to odd number of splines)
I can provide more measurements if needed.
If anyone would be able to help identify which JIS spline spec this is, it would be greatly appreciated.
End goal of this would be to get a DXF and EDM the spline profile.
Thanks!