Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SDETERS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

I'm looking for fatigue material data

Status
Not open for further replies.

Klaus800

Materials
Dec 26, 2016
4
I'm looking for the two steel grades A283C and A572Gr50C (in Germany S235 and S355)the following parameters for the lifetime calculations (FEM calculations of Fatigue/Durability with Siemens NX)

Fatigue Strength Coefficient
Fatigue Strength Exponent
Fatigue Ductility Coefficient
Fatigue Ductility Exponent
Cyclic Strength Coefficient
Cyclic Strain Hardening Exponent


Many thanks for your help and many greetings
Klaus
 
Replies continue below

Recommended for you

For the A572 try:

For the A283C its got higher Mn but
it appears that, according to

it is equivalent to an A36, which would lead one to web page:

I'm not sure about the German standards, but you could try the
T.H.Darmstadt fatigue database. Authors Heuler/Seeger.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor