Impact at high temperature?

Status
Not open for further replies.

bmoorthy

Mechanical
May 29, 2003
457
Is there some thing called high temperature impact test (Say test at 343 deg C), some thing like high temp Tensile strength?

If so what will be guiding standard

Under what circumstance one would specify such test?
 
Replies continue below

Recommended for you

Elevated temperature impact tests are performed to define the location of the upper shelf impact energy for materials. Beyond the upper shelf, impact tests are not that typical, and would provide limited information because of the rapid strain rates involved with Charpy impact testing.

I would recommend a hot tensile or notched hot tensile test and evaluate the loss of ductility (%RA) for the material in question. Certain nickel-base alloys can exhibit a loss of ductility commonly referred to as ductility dip cracking (DDC).
 