Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Impact test requirement of API 650 tank

Status
Not open for further replies.

nsbreddy

Mechanical
Joined
Jan 19, 2012
Messages
12
Location
SA
As I understand, impact test requirements for materials are governed by fig 4-1a unless purchaser has specified the impact test for all thicknesses.
I am using group III materials for my tank design. With MDMT -29 C the maximum thickness I can use without impact test is ~21mm. Is there any other requirements in API 650 I have overlooked?

Help me understand better....
 