Impressed current cathodic protection in tanks already constructed

Status
Not open for further replies.

jor1492

Mechanical
Aug 3, 2015
106
I am in a project where I am seeing tanks already constructed but without cathodic protection system.
Is there a form of implement this system or something that give the cathodic protection to this tanks?
 
Replies continue below

Recommended for you

For cathodic protection of the underside of oil tanks, it may or may not be feasible. One question is whether there's an existing liner under the tank bottom that would insulate it from the ground. If you have to replace the bottom in an existing tank, a cathodic system can be added at that time.

For cathodic protection of the interior of water storage tanks, it is not uncommon to add a system to an existing tank- contact the cathodic suppliers. Easier to do this when the tank is down for repainting or other repair.
 