Hayms

Materials
Nov 3, 2023
7
Hello,

Is there a spec/manual with a method to calculate the maximum bending thinning at the extrados for larger radius induction bends (10D,20D) for liquid or gas lines?
ASME B16.49 Section 12.3 references a 10% thinning. But wouldn't a 6D induction bend have a higher thinning allowance then a 10D Induction Bend?

Details:
NPS 20, API 5L, X65 Pipe MOT: 100F
Design Pressure 1300 psi 0.5 inch WT

Thank you.


 
Replies continue below

Recommended for you

BS PD 8010 quotes bend thinning as 50 divided by n+1, where n is D of the radius.

So a 5D bend is just over 8%.

No idea where 10% comes from.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
"Normal" 40D bends don't normally need any thicker pipe.

10D and 20D is not normally seen.

Usually 3 or 5 induction or 40D cold bends.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 